Material Notes:
Identification: ALLYL ALCOHOL ETHOXYLATECAS: 27274 – 31 – 3Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: MonomerInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 8.00 °C
46.4 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear, Clean Liquid
RPG31
Color <100 HU
Hazen, RPG23
Composition Active
1
Ally Alcohol
<0.1%, RPG99
Hydroxyl Number 109-116 mg KOH/g
RPG06
Ionic Charge Nonionic