Solvay MACKSTAT® GCM Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MACKSTAT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKSTAT® GCM Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackstat GCM is a formaldehyde, paraben and halogen free preservative system that provides broad range protection against gram positive/negative bacteria was well as yeasts and molds. Mackstat GCM combines a safe and globally accepted cosmetic preservative, methylisothiazolinone, with an emollient ester produced from vegetable feedstocks. Mackstat GCM is an easy to handle liquid that disperses readily in cold systems and is effective over a broad pH range. Solubility: Water-Dispersible; Ethanol-Soluble; Propylene Glycol-Soluble; Olive Oil-Dispersible; Butylene Glycol-Soluble; Glycerin-Dispersible; 10% SLES Aqueous Solution-SolubleUses: Hair Conditioners, Shin Care Lotions and ShampooInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.028 g/cc
0.03714 lb/in³
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Color <200
APHA
Composition Methylisothiazolinone
0.9-1.0%