Material Notes:
Product Description: Mackam 2C-LVA is a mild amphoteric foaming and cleansing agent that can reduce the overall irritation of cleansing products into which it is formulated. It is often used as a detoxifying agent in baby shampoos. This material is compatible with anionic, non-ionic and most cationic systems. Mackam 2C-LVA aids in flash foaming and improves the foam stability of most formulations. This particular grade exhibits a significantly lower viscosity than others, making it very easy to empty containers and pump. Infrared Spectrum: Matches StandardINCI NAME: Disodium CocamphodiacetateCAS: 68650-39-5EINECS: 272-043-5Uses: Shampoos and Hand Soaps, Bubble Bath, Body Wash, Remoistened Wipes, Hospital Cleansers and Hard Surface Cleaners.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 46.6 - 54.5 %
46.6 - 54.5 %
Karl Fisher
pH 8.0 - 8.5
8.0 - 8.5
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition Propylene Glycol
Report
Sodium Chloride
10.5-12.5%
Solids,-(NaCl + Propylene Glycol)
35.5-38%
Copyright © lookpolymers.com All Rights Reserved