Solvay IGEPAL® CO 520 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name IGEPAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay IGEPAL® CO 520 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY) ETHANOL, BRANCHEDCAS: 68412-54-4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL® CO-520 is a nonyl phenol ethoxylate (5 moles EO). Emulsifier and coupling agent. Intermediate to anionic surfactants. Emulsifier and coupling agent. Emulsifier/dispersant for universal colorants.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 55-62°C
1% in 15% IPA/Water, RP-0736
Color <100
APHA, RP-0134
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343