Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Adflexâ„¢ KS-021P TPO Resin

Category Polymer , Thermoplastic
Manufacturer LyondellBasell
Trade Name Adflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Adflexâ„¢ KS-021P TPO Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Blown Film/Impact ModificationKey Features: excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable, no slip, no antiblock thermoplastic olefin resinApplications: films, impact modification, toys, lawn and garden equipmentMeets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.Description: Adflex KS-021P thermoplastic olefin resin designed for impact modification of polypropylene, as well as monolayer and multilayer air quenched flown films (no slip, no anitblock). It is based monproprietary Montell process technology. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D792B
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Yield 7.00 MPa
1020 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Elongation at Yield 32 %
32 %
ASTM D638
Flexural Modulus 0.230 GPa
33.4 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Users viewing this material also viewed the following: