Solvay ALKAMULS® S 90 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ALKAMULS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ALKAMULS® S 90 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: SORBITAN MONOISOSTEARATECAS: 71902 – 01 – 7EINECS: 276 – 171 – 2Available in: Asia Pacific, Europe, Latin America and North America.Applications: Water/Oil emulsifier for mineral and vegetable oils in metalworking. Used in oil spill dispersant formulations. Also used in a many industrial emulsion like polyacrylamide emulsions or explosive inverse emulsions.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Optical Properties Metric English Comments
Gardner Color Number <= 13
<= 13
OA-71_1
Chemical Properties Metric English Comments
Total Acid Number <= 8.0
<= 8.0
[mg KOH/g]; ISO 660
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Liquid Clear
OS-500
Composition Active
1
HLB number 5
Hydroxyl Number 215-245 mg KOH/g
OA-086
Ionic Charge Nonionic
Saponification number 143-153 mg KOH/g
OA-031_2