S&E Specialty Polymers TufFill™ 5701 Black PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Calcium Carbonate , Polypropylene, Extrusion Grade
Manufacturer S&E Specialty Polymers
Trade Name TufFill™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill™ 5701 Black PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: High Calcium carbonate filed, high heat resistance thermoplastic extrusion grade based on polypropylene copolymer/homopolymer.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Melt Flow 0.950 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.950 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70.0
70.0
ISO 868
Tensile Strength 21.9 MPa
3180 psi
ISO 527
Elongation at Break 469 %
469 %
ISO 527
Flexural Modulus 2.382 GPa
345.5 ksi
ISO 178
Izod Impact, Notched (ISO) 4.98 kJ/m²

@Temperature -40.0 °C
2.37 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
15.9 kJ/m²

@Temperature 24.0 °C
7.57 ft-lb/in²

@Temperature 75.2 °F
ISO 180/1A
Impact Test 22.4 J
16.5 ft-lb
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75