Solvay AG-RHOâ„¢ FKC 1000 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name AG-RHO™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay AG-RHOâ„¢ FKC 1000 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Biological Activator specifically designed to formulate high load Glyphosate formulation.Identification: SURFACTANT IN WATER SOLUTIONSolubility: Soluble in water. Insoluble in polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Biological activator, wetting agent for herbicide compounds.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% in water; L100
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content 55 - 65 %
55 - 65 %
L020
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Liquid
Ionic Charge Amphoteric