SolVin 367NK Polyvinyl Chloride Medium Viscosity Paste

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Powder
Manufacturer SolVin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SolVin 367NK Polyvinyl Chloride Medium Viscosity Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made by microsuspension polymerization for plastisol preparation. MAIN APPLICATIONS Spread coating : - artificial leather compact layer - artificial leather foam layer. Molding and dipping. Spraying : - Polyurethane sealants. ADVANTAGES - Good acceptance in Polyurethane formulations.Information provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Particle Size 125 µm
125 µm
<0.2 g/kg greater than value; ISO 787-18
Viscosity Measurement 67
67
K value; ISO 1628-2