Material Notes:
Approx. H+ equivalent weight 42.4. Mix Ratio with GY 6010 is 23.Comments/Applications: Pure isophorone diamine used to enhance the workability of coating systems providing longer pot lives and lower viscosities.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity Measurement 13
13
Processing Properties Metric English Comments
Pot Life 50 min
50 min