Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Volatiles 0.10 %
0.10 %
Particle Size 13 µm
13 µm
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Rubber
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
Descriptive Properties Value Comments
INCI Dimethicone/Vinyl Dimethicone Crosspolymer
Shape Sphere