Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Polymer DF-31B PTFE Pelletized Resin

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Shandong Dongyue Polymer Material Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Polymer DF-31B PTFE Pelletized Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Usage: The resin is used to auto press molding and ram extrusion all kinds of rods, pipe etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse to protect from dust, moisture, etc.Transportation: The products are transported according to non-dangerous products. Heat, moisture, freezing and strong shock should be avoided during transportation. Over-bumpiness and compression is apt to make the resin bind together.Conformable with Q/DYG 006-2004Information provided by Shandong Dongyue Polymer Material Co., Ltd
Physical Properties Metric English Comments
Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
Particle Size 500 - 700 µm
500 - 700 µm
Mechanical Properties Metric English Comments
Tensile Strength >= 20.0 MPa
>= 2900 psi
Elongation at Break >= 200 %
>= 200 %
Processing Properties Metric English Comments
Moisture Content <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
For Fabrication Auto press molding and ram extrusion
Powder Flow (g/min) 700
Smoothness & Cleanliness Grade 1: Test impurity quantity that equal or less than 1mm doesn't exceed two
Qualified: Test plate is white and homogeneous, no metal impurities, total impurity quantity <6
Users viewing this material also viewed the following: