Shakespeare NX-203 diameter 0.2 mm Nylon 6 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare NX-203 diameter 0.2 mm Nylon 6 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentNylon 6Moderate ModulusModerate shrinkage Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Elongation at Break 35 %
35 %
Elongation at Yield 10.5 %
10.5 %
at 1.75 g/D
Thermal Properties Metric English Comments
Shrinkage 8.50 %

@Temperature 175 °C
8.50 %

@Temperature 347 °F