Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 20 lb

Category Polymer , Thermoplastic , Nylon
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare CL-10XT Super Tough Nylon Copolymer Fishing Line, 20 lb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Best balance of toughness and strength. Low stretch for fast hook ups. High abrasion resistance. High knot efficiencyInformation provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 786 MPa
>= 114000 psi
29 lb. Minimum Tensile Load 0.018 in. Diameter
Elongation at Break 25 - 35 %
25 - 35 %