Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: General molding articles; Packing material for industrial parts; and Returnable containers for electronic parts.Information provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0250 g/cc
0.000903 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.4133 MPa
59.94 psi
ASTM D3575
Elongation at Break 8.8 %
8.8 %
ASTM D3575
Flexural Strength 0.2718 MPa
39.42 psi
ASTM D790
Flexural Modulus 0.012036 GPa
1.7457 ksi
ASTM D790
Compressive Strength 0.1851 MPa

@Strain 25.0 %
26.84 psi

@Strain 25.0 %
ASTM D3575
0.2483 MPa

@Strain 50.0 %
36.01 psi

@Strain 50.0 %
ASTM D3575
0.5041 MPa

@Strain 75.0 %
73.12 psi

@Strain 75.0 %
ASTM D3575
Compression Set 44 %
44 %
ASTM D3575
Descriptive Properties Value Comments
Color White
Range of center value of pre-expanded particles 0.14-0.2 in
Users viewing this material also viewed the following: