Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | Minimum |
SYNTHOS Koplen® 0207 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thin walled products.Specific Characteristics: Flammability according .. |
|||
Bulk Density | 0.0250 - 0.0600 g/cc | 0.000903 - 0.00217 lb/in³ | Typical |
SYNTHOS Koplen® 0207 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thin walled products.Specific Characteristics: Flammability according .. |
|||
Bulk Density | >= 0.0250 g/cc | >= 0.000903 lb/in³ | Typical |
SYNTHOS Koplen® 0207 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to thin-wall moldings. Lower density can be achie.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | Minimum |
SYNTHOS Koplen® 0814 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | Minimum |
SYNTHOS Koplen® 0822 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to molded bricks and blocks. Lower density can be.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | Minimum |
SYNTHOS Koplen® 2040 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LP-40E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LSP-40EB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN SP-40D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN SP-40E Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN TOPF-40DB Flame Retardant Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0250 g/cc | 0.000903 lb/in³ | After expansion |
Sekisui PIOCELAN TOPF-40DUB Black (Low VOC, Low odor) Flame Retardant Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |