Seals Eastern 5407 Nitrile Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5407 Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose Nitrile; Peroxide curedInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 73
>= 73
ASTM D2240, Type A
76
76
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 10.34 MPa
>= 1499 psi
ASTM D412 Method A
16.91 MPa
2453 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield 1.93 MPa
280 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 2.42 MPa
>= 351 psi
Stress at Elongation M50; ASTM D412 Method A
3.56 MPa
516 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 5.18 MPa
>= 751 psi
Stress at Elongation M100; ASTM D412 Method A
9.301 MPa
1349 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 71 %
>= 71 %
ASTM D412 Method A
144 %
144 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.01322 GPa
1.918 ksi
ASTM D412 Method A
Shear Modulus 0.00436 GPa
0.632 ksi
ASTM D412 Method A
Secant Modulus 0.01243 GPa
1.803 ksi
ASTM D412 Method A
Tear Strength Test 99
99
(psi); ASTM D624, Die B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 28