Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5400 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5401 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5407 Nitrile Rubber General purpose Nitrile; Peroxide curedInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5433 Nitrile Rubber General purpose Nitrile; Low water swellInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5484 Nitrile Rubber Low temperature service NitrileInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5403 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
Seals Eastern 5404 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |