Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
ASTM D792
Melt Flow 28 g/10 min

@Load 2.16 kg,
Temperature 250 °C
28 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 123 MPa
17800 psi
5 mm/min; ASTM D638
Flexural Strength 177 MPa
25700 psi
2.8 mm/min; ASTM D638
Flexural Modulus 8.83 GPa
1280 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.686 J/cm

@Thickness 3.17 mm
1.29 ft-lb/in

@Thickness 0.125 in
ASTM D256