Material Notes:
Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specification Qualifications:Satisfies Type III for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ResinSatisfies Class 5, Form P for SAE AMS 3644G: Polyimide, Molded Rod, Bar and Tube, Plaque, and Formed PartsSatisfies Type III for MIL-R-46198: Resin, Polyimide, Hot Pressed or Pressed and SinteredInformation provided by Saint-Gobain Performance Plastics
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 63.4 MPa
9200 psi
ASTM D638
Elongation at Break 5.5 %
5.5 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Compressive Yield Strength 25.5 MPa

@Strain 1.00 %
3700 psi

@Strain 1.00 %
ASTM D695
117 MPa

@Strain 10.0 %
17000 psi

@Strain 10.0 %
ASTM D695
Compressive Modulus 2.50 GPa
363 ksi
ASTM D695