Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material

Category Ceramic , Glass , Glass Fiber
Manufacturer Saint-Gobain Quartz PLC
Trade Name Chemfab® TCK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid fiber that offers an extremely high strength-to-weight ratio. TCK is an excellent fabric for use in high moisture environments, for applications subjected to severe flexing, or for when added durability is required.Dimensional Stability: The Kevlar® base of TCK keeps stretch or shrinkage to less than 1% under normal operating tensions (3 to 10 pounds per inch of width) and temperatures up to 500°F. TCK belting has excellent resistance to flex fatigue.Release Properties: The release properties of TCK exceed those of any other available belting material. TCK has a low coefficient of friction.Chemically Resistant: The PTFE coating encapsulates the Kevlar® belting carcass and enhances its useful service life.Light Weight: The inherent strength of the Kevlar® filament provides durable belting at a fraction of the weight of other materials. Less power is required to move TCK belting (and the products moved).High Strength: Kevlar®, the filament base of the belting carcass, is stronger than steel on a pound-for-pound basis.Flex Fatigue Resistant: The strength of TCK, combined with its excellent flex fatigue properties, means TCK belting can be used on small pulley diameters for a long in-use life span.High Thermal Capability: At temperatures of up to 500°F, TCK belting continues to maintain its high performance profile.Low Thermal Mass: TCK belting (including the seam areas) quickly dissipates heat with low heat sink properties.Fabrication Technology: Saint-Gobain Performance Plastics belt seams have been specifically engineered to reduce the flex fatigue failure. Substantially reduced flex fatigue means longer belt life.Notes on TCK® 1590 Leno Weave Open Mesh Belting Material: TCK 1590 is a high strength belting product. It is a Leno weave, open mesh material intended for use in force hot air dryers. Substrate is Kevlar®. The substrate is coated with PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.03 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.2671 - 0.3114 g/cc
0.009647 - 0.01125 lb/in³
Mechanical Properties Metric English Comments
Elongation at Yield <= 1.0 %
<= 1.0 %
Value given for Elongation at a loading of 40 lbs/in
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Fill)
70.1 kN/m
400 pli
Tensile Strength (Warp)
Descriptive Properties Value Comments
Weight (oz/yd^2) 6.5