| Category | Other Engineering Material |
| Manufacturer | SMAC |
| Trade Name | SMACWRAP® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SMAC SMACWRAP® EX Damping Material, 0.20 mm.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 2000 microns | 78.7 mil |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Abrasion | 0.44 <br>@Temperature -10.0 °C |
0.44 <br>@Temperature 14.0 °F |
Loss Factor |
| 0.90 <br>@Temperature -20.0 °C |
0.90 <br>@Temperature -4.00 °F |
Loss Factor | |
| 0.97 <br>@Temperature -40.0 °C |
0.97 <br>@Temperature -40.0 °F |
Loss Factor | |
| 1.2 <br>@Temperature -25.0 °C |
1.2 <br>@Temperature -13.0 °F |
Loss Factor | |
| 1.4 <br>@Temperature -35.0 °C |
1.4 <br>@Temperature -31.0 °F |
Loss Factor |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Delta | 13 dB | 4000 HZ |
| 6.5 dB | 250 Hz | |
| 7 dB | 1000 Hz | |
| 8.8 dB | 2000 Hz | |
| 9 dB | 125 Hz | |
| 9.5 dB | 500 Hz | |
| Surface Mass | 200 g/sqm |