SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI) + PCE
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 6.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
6.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.0 MPa
9860 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 80 %
80 %
Type I, 5 mm/min; ASTM D 638
Flexural Yield Strength 106 MPa
15400 psi
2.6 mm/min, 100 mm span; ASTM D 790
Flexural Modulus 2.53 GPa
367 ksi
2.6 mm/min, 100 mm span; ASTM D 790
Izod Impact, Notched 3.73 J/cm

@Temperature 23.0 °C
6.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 20.82 J/cm

@Temperature 23.0 °C
39.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157 °C

@Thickness 6.40 mm
315 °F

@Thickness 0.252 in
unannealed; ASTM D 648
UL RTI, Electrical 115 °C
239 °F
UL 746B
UL RTI, Mechanical with Impact 115 °C
239 °F
UL 746B
UL RTI, Mechanical without Impact 115 °C
239 °F
UL 746B
Flammability, UL94 HB

@Thickness 0.760 mm
HB

@Thickness 0.0299 in
UL 94
Electrical Properties Metric English Comments
Comparative Tracking Index 175 - 250 V
175 - 250 V
PLC code 3; UL 746A
Hot Wire Ignition, HWI 60 - 120 sec
60 - 120 sec
PLC code 1; UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
surface, PLC code 0; UL 746A