Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Notched | 3.73 J/cm @Temperature 23.0 °C |
6.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® PPC4701 PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 3.73 J/cm @Temperature 23.0 °C |
6.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 3.73 J/cm @Temperature 23.0 °C |
6.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SPN410 PPE+PS Improved productivity. 210F (99C) DTUL. UL94 HB rated. |
|||
Izod Impact, Notched | 3.73 J/cm @Temperature 23.0 °C |
6.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 3.73 J/cm @Temperature 23.0 °C |
6.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |