Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL N190 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL N190 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE/PS, 90 oC, FR V0
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 29.8 g/10 min

@Load 10.0 kg,
Temperature 250 °C
29.8 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
SABIC - Japan Method
Elongation at Break 76 %
76 %
SABIC - Japan Method
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.26 GPa
328 ksi
ASTM D790
Izod Impact, Notched 2.83 J/cm
5.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
5VA

@Thickness 2.80 mm
5VA

@Thickness 0.110 in
UL 94
Users viewing this material also viewed the following: