SABIC Innovative Plastics NORYL EM7301F PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EM7301F PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% glass-reinforced. HDT 252F. Good flow and polyurethane foam adhesion. Black only.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.0 MPa
9860 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 96.0 MPa
13900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.64 GPa
528 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 122 °C

@Thickness 6.40 mm
252 °F

@Thickness 0.252 in
unannealed; ASTM D648