Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* NF001 is a compound based on PC+ABS Blend resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Tensile Modulus 3.65 GPa
529 ksi
50 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 3.65 GPa
529 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.79 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 123 °C

@Thickness 3.20 mm
253 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: