Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.65 GPa | 529 ksi | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6/66 FRC 3 TS PA6/66 flame retarded, heat stabilized PA 6 + PA 66 alloy for injection molding, reinforced with 30 % glass fiber, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 5 a.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the .. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | 51 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS (Asia Pacific) LNP* Lubricomp* ZFL31XXC is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM Data |
Styron CALIBRE™ 7101 15 Polycarbonate, 10% Glass Reinforced CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM Data |
Styron CALIBRE™ 7101 8 Polycarbonate, 10% Glass Reinforced CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific) LNP* Thermocomp* NF001 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Tensile Modulus | 3.65 GPa | 529 ksi | ASTM D638 |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |