SABIC Innovative Plastics LNP COLORCOMP D1000FL PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP D1000FL PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* COLORCOMP* D1000FL is an unfilled compound based on Polycarbonate resin. Added features of this grade are: Superior Molding, Low Extractible.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.300 %
0.300 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
Type I, 5 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 2.39 GPa
347 ksi
50 mm/min; ASTM D638
Thermal Properties Metric English Comments
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af