SABIC HC100 Crystalline Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC HC100 Crystalline Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: HC100 is a crystalline, high molecular weight thermoplastic polymer made by a continuous melt-phase polymerization process followed by solid-state polymerization.Characteristics: HC100 is a specially formulated PET grade that is characterized by High I.V. The High I.V. confers good mechanical properties.Typical Applications: This PET grade is especially used for woven tape fabric, involved in making sacks, geotextiles, carpet backing, composites and other non-bottle applications.Information provided by SABIC.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
crystalline density; SABIC (IRC0032)
Viscosity Test 82 - 86 cm³/g
82 - 86 cm³/g
Intrinsic; SABIC (IRC0041)
Maximum Moisture Content <= 0.35
<= 0.35
% w/w; SABIC (IRC0050)
Thermal Properties Metric English Comments
Melting Point 240 - 260 °C
464 - 500 °F
SABIC (IRC0053)
Descriptive Properties Value Comments
Color (b) -1.5 ± 2.0
Color (L) 89 ± 4.0
DEG Content = 1.2 % w/w
SABIC (IRC0055)
Dust Content < 0.01 % w/w
SABIC (IRC0060)