Ritelok GM18 Aluminum Parts Gasket Maker

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok GM18 Aluminum Parts Gasket Maker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. Flexible gasket maker for aluminum flanges. Replaces pre-cut gaskets, Does not shrink or relax, flexible, Withstands temperatures from 65°F to 300°F (55°C)-150°C), Thixotropic formulation, Fills scratches and gouges
Physical Properties Metric English Comments
Viscosity 750000 - 3.75e+6 cP
750000 - 3.75e+6 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Descriptive Properties Value Comments
Maximum Gap Fill 0.25 mm
Higher with primer