Material Notes:
UV 408 is a low viscosity, high clarity, UV curing adhesive with excellent adhesion to glass. The product is well suited for bonding close fitting parts and has excellent moisture resistance.Applications: Lens bonding, Glass assembly, Fiber optic bonding.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Viscosity 50 - 100 cP

@Temperature 25.0 °C
50 - 100 cP

@Temperature 77.0 °F
Uncured
Thickness <= 6350 microns
<= 250 mil
Cured film
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Cured
Tensile Strength at Break 46.9 MPa
6800 psi
Cured
Elongation at Break 10 %
10 %
Cured
Thermal Properties Metric English Comments
CTE, linear 166 µm/m-°C

@Temperature 20.0 °C
92.2 µin/in-°F

@Temperature 68.0 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Shrinkage 8.0 %
8.0 %
Upon cure
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Descriptive Properties Value Comments
Color Clear
Composition Urethane Oligomer/ (Meth) Acrylate
Solubility Isopropyl Alcohol, Chlorinated solvents
Toxicity Low
Water Resistance 4 hours
Cured, 1/4" x 1/4", boiling water, substrate failure