Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 166 µm/m-°C @Temperature 20.0 °C |
92.2 µin/in-°F @Temperature 68.0 °F |
Cured |
Resin Technology Group UV-408 Low-Viscosity, High Clarity, UV Curable Adhesive UV 408 is a low viscosity, high clarity, UV curing adhesive with excellent adhesion to glass. The product is well suited for bonding close fitting parts and has excellent moisture resistance.Applica.. |
|||
CTE, linear | 166 µm/m-°C @Temperature 20.0 °C |
92.2 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |
|||
CTE, linear | 166 µm/m-°C @Temperature 20.0 °C |
92.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
CTE, linear | 166 µm/m-°C | 92.2 µin/in-°F | Above Tg |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |