Material Notes:
REPOL Polypropylene H200MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H200MK is recommended for use in injection molding processes. It is an ideal material for molding syringes and clear rigid articles with intricate, long flow paths and multicavity molding. Repol H200MK contains clarifier and antistatic agent that reduces static charge build up on products. Features: Low static charge build-up and reduced dust pickupImproved clarityGood flow behaviorConsistent processabilityExcellent stiffness and color stabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
50mm/min; ASTM D638
Elongation at Yield 11 %
11 %
50mm/min; ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.260 J/cm

@Temperature 23.0 °C
0.487 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648