Material Notes:
QC-2150 is a glass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150 is recommended for applications such as aircraft interiors and public transportation components requiring composite materials having very low flammability, low smoke, and minimal generation of toxic gasses.Form = Rolled SheetColor = Natural, BlackGlass Fiber Content = 50% nominalInformation provided by Quantum Composites.
Physical Properties Metric English Comments
Specific Gravity 1.82 g/cc
1.82 g/cc
ASTM D792
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 227 MPa
32900 psi
ASTM D638
Flexural Strength 358 MPa
51900 psi
ASTM D790
Flexural Modulus 21.0 GPa
3050 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Shelf Life 2.00 Month

@Temperature 4.44 °C
2.00 Month

@Temperature 40.0 °F
6.00 Month

@Temperature -17.8 °C
6.00 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Fiber Length (in) 1
Glass, nominal