Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 2.00 Month @Temperature 4.44 °C |
2.00 Month @Temperature 40.0 °F |
|
Quantum Composites AMC™ 2593 45% Carbon Fiber Reinforced Phenolic SMC AMC™ 2593 (126-40-139) is a carbon fiber reinforced phenolic engineered structural composite molding compound. The carbon fiber is PAN based 3K standard modulus tow. It exhibits outstanding low f.. |
|||
Shelf Life | 2.00 Month @Temperature 4.44 °C |
2.00 Month @Temperature 40.0 °F |
|
Quantum Composites QC-2150 50% Glass Reinforced Phenolic SMC QC-2150 is a glass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150 is recommended for applications such as a.. |
|||
Shelf Life | 2.00 Month @Temperature 4.44 °C |
2.00 Month @Temperature 40.0 °F |
|
Quantum Composites QC-2150LD NT 25% Fiberglass Reinforced Phenolic SMC QC-2150LD NT (126-40-50) is a fiberglass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150LD NT (126-40-50) is.. |