Premix Thermoplastics PREBLACK CP 731-40 Black Universal Masterbatch, 40% Carbon Black

Category Polymer , Thermoplastic
Manufacturer Premix Thermoplastics Inc.
Trade Name PREBLACK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREBLACK CP 731-40 Black Universal Masterbatch, 40% Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PREBLACK CP 731-40 black universal masterbatch has been developed for the colouring of injection moulded and extruded products made e.g. out of polyolefines, polystyrenes, ABS, PVC, PA, PC and POM. Due to the good homogeneity of PREBLACK CP 731-40, it is well suited for demanding applications. According to BgVV regulations PREBLACK CP 731-40 is approved for use in contact with foodstuffs, as long as the carbon black content of the produced product is less than 2.5 %. Dosing .5-10% depending on desired blackness.Information from Premix OY
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
when produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Light Fastness 8
Very Good