Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymax® Maxelast® C49C10 TPE, Transparent

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Nagtong Polymax
Trade Name Maxelast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymax® Maxelast® C49C10 TPE, Transparent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.872 g/cc
0.872 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 10

@Time 10.0 sec
10

@Time 0.00278 hour
ASTM D2240
Tensile Stress 0.0400 MPa

@Strain 100 %
5.80 psi

@Strain 100 %
ASTM D412
0.0800 MPa

@Strain 300 %
11.6 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield >= 0.480 MPa
>= 69.6 psi
ASTM D412
Elongation at Break >= 1300 %
>= 1300 %
ASTM D412
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved