Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C49C15 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® P3908T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® P3955T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ISO 1183 |
Nanocyl PLASTICYL™ PP2001 Polypropylene - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C4900 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C4902 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C4903 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C4905 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C4907 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D792 |
Polymax® Maxelast® C49C10 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 7500 Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | ASTM D1505 |
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 7500 Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Specific Gravity | 0.872 g/cc | 0.872 g/cc | |
ExxonMobil Mobil Clean 10W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |