PolyOne Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ HTE 3060 Polyvinyl Chloride + NBR (PVC+NBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons and oils, offer excellent weatherability, and are an economical alternative to thermoset rubber and other more costly thermoplastic elastomers.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Melt Flow 26 g/10 min

@Load 5.00 kg,
Temperature 190 °C
26 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
15 sec; ASTM D2240
Tensile Strength at Break 14.0 MPa
2030 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 3.74 MPa

@Strain 100 %
542 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
8.85 MPa

@Strain 300 %
1280 psi

@Strain 300 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 460 %
460 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 30.1 kN/m
172 pli
Die C, 510 mm/min; ASTM D624
Compression Set 49 %

@Temperature 70.0 °C,
Time 79200 sec
49 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395A
58 %

@Temperature 100 °C,
Time 79200 sec
58 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395A
Thermal Properties Metric English Comments
Brittleness Temperature -59.0 °C
-74.2 °F
ASTM D746
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Forms Pellets
Generic Material PVC+NBR
Generic Name Polyvinyl Chloride + NBR (PVC+NBR)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
General Purpose
Industrial Applications