Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4466 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4466 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466 is available in black or brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Water Absorption 0.179 %
0.179 %
ASTM D570
Linear Mold Shrinkage 0.0076 cm/cm
0.0076 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 73
73
ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 0.58 %
0.58 %
ASTM D638
Tensile Modulus 10.3 GPa
1490 ksi
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 8.80 GPa
1280 ksi
ASTM D790
Compressive Strength 156 MPa
22600 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM D638
Shear Modulus 3.84 GPa
557 ksi
Calculated
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.182 J/cm²
0.866 ft-lb/in²
ASTM D256
Impact 98
98
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.540 W/m-K

@Temperature 100 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 202 °C
396 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 27.4 %
27.4 %
ASTM D2863
Shrinkage 0.271 %
0.271 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+11 ohm-cm
2.00e+11 ohm-cm
ASTM D247
Dielectric Constant 5.7
5.7
ASTM D150
Dielectric Strength 10.6 kV/mm
269 kV/in
Short Time; ASTM D149
Dissipation Factor 0.067
0.067
ASTM D150
Arc Resistance 182 sec
182 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved