Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | JIS-K-6249/ASTM D257 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Volume Resistivity | >= 2.00e+11 ohm-cm | >= 2.00e+11 ohm-cm | |
LG Chemical LGflex GL100 Plasticizer Features: Excellent Heat Loss and Non-endocrine disrupter Application: PVC Power Cable, SheetsInformation provided by LG Chemical |
|||
Volume Resistivity | >= 2.00e+11 ohm-cm | >= 2.00e+11 ohm-cm | |
LG Chemical LGflex GL300 Plasticizer Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical |
|||
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | ASTM D247 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | ASTM D247 |
Plenco 7487 Phenolic, Granular, Transfer Molded PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple.. |
|||
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | IEC 60093 |
Polyplastics Duranex® 7300E Polybutylene Terephthalate (PBT), Conductive, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | cured 3 hrs @ 74°C |
Tra-Con Tra-Bond 724-5 Low Viscosity Polyurethane Adhesive TRA-BOND 724-5 is a premixed and frozen, electrically insulating, polyurethane adhesive. This resilient adhesive exhibits good adhesion to a wide variety of substrates, including aluminum, solder, n.. |
|||
Volume Resistivity | >= 2.00e+11 ohm-cm | >= 2.00e+11 ohm-cm | |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Volume Resistivity | 2.00e+11 ohm-cm | 2.00e+11 ohm-cm | ASTM D247 |
Plenco 7321 Phenolic, Nodular, Compression Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |