Plansee TaKS Grain Stabilized Tantalum

Category Metal , Nonferrous Metal , Refractory Metal
Manufacturer Plansee SE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee TaKS Grain Stabilized Tantalum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tantalum with silicon as a doping agent - sintered and grain stabilizedCharacteristics:Very high thermal stability - annealing temperatures up to ~ 2000°CFine-grained microstructureHigh ductilityHigh strengthAvailable as wire or sheet, suitable for sintering into tantalum anodes or for furnace construction applications.Information provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 16.6 g/cc
16.6 g/cc
Component Elements Properties Metric English Comments
Silicon, Si <= 0.10 %
<= 0.10 %
Tantalum, Ta >= 99.9 %
>= 99.9 %