Polymer Property : Specific Gravity = 16.6 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 16.6 g/cc
16.6 g/cc
Plansee TaKS Grain Stabilized Tantalum
Tantalum with silicon as a doping agent - sintered and grain stabilizedCharacteristics:Very high thermal stability - annealing temperatures up to ~ 2000°CFine-grained microstructureHigh ductilityHi..
Specific Gravity 16.6 g/cc
16.6 g/cc
H.C. Starck NRC® 3N5 (UNS R05200) Electron Beam Melted Tantalum
Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio..
Specific Gravity 16.6 g/cc
16.6 g/cc
H.C. Starck NRC® 4N (UNS R05200) Electron Beam Melted Tantalum
Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio..
Specific Gravity 16.6 g/cc
16.6 g/cc
H.C. Starck NRC® 4N5 (UNS R05200) Electron Beam Melted Tantalum
Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio..
Specific Gravity 16.6 g/cc
16.6 g/cc
H.C. Starck NRC® 5N (UNS R05200) Electron Beam Melted Tantalum
Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio..
Specific Gravity 16.6 g/cc
16.6 g/cc
H.C. Starck NRC® Tantalum (UNS R05200)
Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di..