Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pasargad Polymer Peyvand Pasalen 3P-H3130B Polypropylene, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Pasargad Polymer Peyvand
Trade Name Pasalen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pasargad Polymer Peyvand Pasalen 3P-H3130B Polypropylene, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 4.40 GPa
638 ksi
ISO 527-2
Charpy Impact Unnotched 4.80 J/cm²
22.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
Unannealed; ISO 75-2/C
Descriptive Properties Value Comments
Color Black