Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-2
Elongation at Break 60 %
60 %
ISO 527-2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 230 °C
446 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ISO 75-2/C
Descriptive Properties Value Comments