Parker Chomerics CHO-BOND 1076 Part B Organoplatinum Compound

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1076 Part B Organoplatinum Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 0.960 g/cc
>= 0.960 g/cc
Thermal Properties Metric English Comments
Flash Point >= 46.00 °C
>= 114.8 °F
Descriptive Properties Value Comments
Color Straw
Physical Form Straw colored liquid slight odor
Platinum Siloxane Complex wt. % Max 5
Silicone Resin % >60
Tetramethyldivinyl disiloxane wt. % Max 15