Parker Chomerics C-Wing™ Heat Spreader

Category Ceramic
Manufacturer Parker Chomerics
Trade Name C-Wing™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics C-Wing™ Heat Spreader.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. C-Wing spreaders are a ceramic version which are available for EMI-sensitive applications.Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 1520 microns
60.0 mil
Thermal Properties Metric English Comments
Thermal Conductivity 26.0 W/m-K
180 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color Tan
Pressure-sensitive adhesive system Silicon-Based THERMATTACH
Thermal Conductor Aluminum Oxide (std.) / Acrylic (new)