Parabeam Industrie Paraglass 5 3D Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Core Material , Composite Fibers
Manufacturer Parabeam Industrie
Trade Name Paraglass
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parabeam Industrie Paraglass 5 3D Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklay one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechanical properties. Parabeam® can be used for many applications in the composite industry while offering multiple advantages against traditional sandwiches and solid laminates such as woods, foams, balsa, honeycombs and more. Information provided by the manufacturer, Parabeam Industrie, The Netherlands.
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 3.70 MPa
>= 537 psi
ASTM C365
4.80 MPa
696 psi
ASTM C365
Shear Modulus >= 0.00760 GPa
>= 1.10 ksi
ASTM C273
0.00950 GPa
1.38 ksi
Typical; ASTM C273
Shear Strength >= 0.700 MPa
>= 102 psi
ASTM C273
0.800 MPa
116 psi
Typical; ASTM C273
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K
0.416 BTU-in/hr-ft²-°F
DIN 52616