Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 116 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.800 MPa
116 psi
Typical; ASTM C273
Parabeam Industrie Paraglass 5 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklay one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechan..
Shear Strength 0.800 MPa
116 psi
ASTM C273
SABIC Innovative Plastics ULTEM Foam XP060 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Shear Strength 0.800 MPa
116 psi
Plate Shear, L direction
Hexcel® HexWeb® CRF-3/8-ACG-.002-2.3 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Shear Strength >= 0.800 MPa
>= 116 psi
ISO 1922
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Shear Strength 0.800 MPa
116 psi
average; ISO 1922
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Shear Strength 0.800 MPa
116 psi
average; ISO 1922
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Shear Strength 0.800 - 128 MPa
116 - 18600 psi
Average value: 78.5 MPa Grade Count:18
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Copyright © lookpolymers.com All Rights Reserved